Optical constants of SUMITA - Glasses for precision molding
K-PSFn2

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.7699503-1.3004151\text{×}10^{-2}λ^{2}+7.2310519\text{×}10^{-2}λ^{-2}+3.5123072\text{×}10^{-3}λ^{-4}-1.0361594\text{×}10^{-5}λ^{-6}+3.8615781\text{×}10^{-5}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-