Optical constants of SUMITA - Glasses for precision molding
K-PFK85

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.1858326-5.0155632\text{×}10^{-3}λ^{2}+7.5107775\text{×}10^{-3}λ^{-2}+1.7770562\text{×}10^{-4}λ^{-4}-1.2164148\text{×}10^{-5}λ^{-6}+6.1341005\text{×}10^{-7}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book