Optical constants of SUMITA - Glasses for precision molding
K-PBK50

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.2879519-1.0513752\text{×}10^{-2}λ^{2}+1.0963175\text{×}10^{-2}λ^{-2}+2.7027054\text{×}10^{-4}λ^{-4}-1.7054549\text{×}10^{-5}λ^{-6}+1.0857039\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book