Optical constants of SUMITA - Glasses for precision molding
K-LaFK60

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.6248172-1.0251149\text{×}10^{-2}λ^{2}+1.43793\text{×}10^{-2}λ^{-2}+2.4017461\text{×}10^{-4}λ^{-4}-1.041901\text{×}10^{-6}λ^{-6}+1.0237991\text{×}10^{-7}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

References

Sumita Optical Glass Data Book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SUMITA Optical Glass, Inc.

SUMITA Optical Glass, Inc. is a Japanese glass manufacturer

External links


Glass