K-GFK68

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.4994867-5.9285872\text{×}10^{-3}λ^{2}+1.2743526\text{×}10^{-2}λ^{-2}+1.5469636\text{×}10^{-4}λ^{-4}+3.9947612\text{×}10^{-6}λ^{-6}-1.760356\text{×}10^{-7}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-