Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.4804566-1.071977\text{×}10^{-2}λ^{2}+1.35632\text{×}10^{-2}λ^{-2}+3.4918608\text{×}10^{-4}λ^{-4}-2.3041786\text{×}10^{-5}λ^{-6}+1.5937217\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]