Optical constants of SUMITA - Glasses for precision molding
K-CD120

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.8630662-1.1977981\text{×}10^{-2}λ^{2}+3.2706279\text{×}10^{-2}λ^{-2}+1.6821116\text{×}10^{-3}λ^{-4}-7.4783483\text{×}10^{-5}λ^{-6}+1.4696883\text{×}10^{-5}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

References

Sumita Optical Glass Data Book