Optical constants of SUMITA - SFLD
K-SFLD5

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.7102301-1.0851642\text{×}10^{-2}λ^{2}+2.9534854\text{×}10^{-2}λ^{-2}+4.1107114\text{×}10^{-4}λ^{-4}+9.7348452\text{×}10^{-5}λ^{-6}+8.8402787\text{×}10^{-7}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

Sumita Optical Glass Data Book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SF5 optical glass

SF5 is a popular optical glass. Most glass makers produce this or very similar glass under slightly different names.

SF5 and similar glasses produced by different makers

Maker Glass
Schott N-SF5
Hikari E-SF5
HOYA E-FD5
Sumita K-SFLD5
CDGM ZF2