Optical constants of SUMITA - SFLD
K-SFLD2

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.6390073-1.1704695\text{×}10^{-2}λ^{2}+2.4198189\text{×}10^{-2}λ^{-2}+1.25366\text{×}10^{-3}λ^{-4}-5.1544035\text{×}10^{-5}λ^{-6}+7.7549405\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book