Optical constants of SUMITA - SFLD
K-SFLD10

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.8794157-1.2203687\text{×}10^{-2}λ^{2}+3.351206\text{×}10^{-2}λ^{-2}+1.8761149\text{×}10^{-3}λ^{-4}-9.8708915\text{×}10^{-5}λ^{-6}+1.7667333\text{×}10^{-5}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-