Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaKn12

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.9410903-1.1791679\text{×}10^{-2}λ^{2}+2.2466126\text{×}10^{-2}λ^{-2}+3.4761977\text{×}10^{-4}λ^{-4}-1.7639536\text{×}10^{-6}λ^{-6}+1.0304373\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

Sumita Optical Glass Data Book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]