Optical constants of SUMITA - LaK (Lanthanum crown)
K-LaK13

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.8106459-1.0211215\text{×}10^{-2}λ^{2}+2.047301\text{×}10^{-2}λ^{-2}+9.7897189\text{×}10^{-5}λ^{-4}+3.378933\text{×}10^{-5}λ^{-6}-1.1893964\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-