RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SUMITA - LaF (Lanthanum flint)
K-LaFn9

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.0328710-1.386928\text{×}10^{-2}λ^{2}+2.3554889\text{×}10^{-2}λ^{-2}+2.4226145\text{×}10^{-3}λ^{-4}-2.5576787\text{×}10^{-4}λ^{-6}+1.7912149\text{×}10^{-5}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-