Optical constants of SUMITA - LaF (Lanthanum flint)
K-LaFn2

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.8209581-1.2387214\text{×}10^{-2}λ^{2}+1.929917\text{×}10^{-2}λ^{-2}+1.0436756\text{×}10^{-3}λ^{-4}-7.7921095\text{×}10^{-5}λ^{-6}+5.1365409\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book