Optical constants of SUMITA - LaF (Lanthanum flint)
K-LaF3

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.8849358-1.2668322\text{×}10^{-2}λ^{2}+2.1170498\text{×}10^{-2}λ^{-2}+8.5117754\text{×}10^{-4}λ^{-4}-4.902482\text{×}10^{-5}λ^{-6}+3.7361709\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

Sumita Optical Glass Data Book