Optical constants of SUMITA - BaSF (Barium dense flint)
K-BaSF12

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.7201325-1.2755345\text{×}10^{-2}λ^{2}+2.235917\text{×}10^{-2}λ^{-2}+1.1060351\text{×}10^{-3}λ^{-4}-5.6019485\text{×}10^{-5}λ^{-6}+5.8998558\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-