RefractiveIndex.INFO

Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - Obsolete glasses
LASFN9

Wavelength: µm
 (0.365 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.97888194λ^2}{λ^2-0.0118537266}+\frac{0.320435298λ^2}{λ^2-0.052738177}+\frac{1.92900751λ^2}{λ^2-166.25654}$$

Conditions & Spec sheet

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 9.44e-07 1.14e-08 -1.87e-11 9.22e-07 1.22e-09 0.255
n_d: 1.85025
V_d: 32.17
glass_code: 850322.444
glass_status: preferred
density: 4.44 g/cm3
coefficient_of_thermal_expansion_1: 7.4e-06 K-1
coefficient_of_thermal_expansion_2: 8.4e-06 K-1
ΔP_gF: 0.0036
climatic_resistance: 2.0
stain_resistance: 0.0
acid_resistance: 2.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

Comments

was replaced by N-LASF9

References

SCHOTT Zemax catalog 2015-07-22

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SCHOTT AG

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links


Glass

External links