RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - Inquiry glasses
N-SF64

Wavelength: µm
 (0.37 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.59163762λ^2}{λ^2-0.0118623434}+\frac{0.219908428λ^2}{λ^2-0.0594585499}+\frac{1.46929315λ^2}{λ^2-133.310762}$$

Comments

inquiry glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -2.06e-06 9.78e-09 -1.67e-11 8.67e-07 1.23e-09 0.279
n_d: 1.70591
V_d: 30.23
glass_code: 706302.299
glass_status: special
density: 2.989 g/cm3
coefficient_of_thermal_expansion_1: 8.48e-06 K-1
coefficient_of_thermal_expansion_2: 9.78e-06 K-1
ΔP_gF: 0.0099
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 1.2
phosphate_resistance: 1.0

References

SCHOTT Zemax catalog 2015-07-22

More info - wiki