Optical constants of SCHOTT - Inquiry glasses
N-PSK53

Wavelength: µm
 (0.31 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.3434087λ^2}{λ^2-0.00675074317}+\frac{0.241417935λ^2}{λ^2-0.0219910513}+\frac{0.952896897λ^2}{λ^2-103.551457}$$

Comments

inquiry glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -9.29e-06 5.78e-09 8.87e-13 4.59e-07 5.86e-10 0.155
n_d: 1.62014
V_d: 63.48
glass_code: 620635.360
glass_status: special
density: 3.6 g/cm3
coefficient_of_thermal_expansion_1: 9.4e-06 K-1
coefficient_of_thermal_expansion_2: 1.09e-05 K-1
ΔP_gF: 0.0053
climatic_resistance: 2.0
stain_resistance: 1.0
acid_resistance: 52.3
alkali_resistance: 1.2
phosphate_resistance: 4.3

References

SCHOTT Zemax catalog 2015-07-22