Optical constants of SCHOTT - Inquiry glasses
N-LAF3

Wavelength: µm
 (0.35 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.73155854λ^2}{λ^2-0.00953833914}+\frac{0.150874455λ^2}{λ^2-0.0407887211}+\frac{1.06586596λ^2}{λ^2-98.0758545}$$

Conditions & Spec sheet

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -2.35e-06 1.07e-08 -9.38e-12 5.72e-07 6.01e-10 0.22
n_d: 1.717
V_d: 47.96
glass_code: 717480.414
glass_status: special
density: 4.14 g/cm3
coefficient_of_thermal_expansion_1: 7.6e-06 K-1
coefficient_of_thermal_expansion_2: 8.7e-06 K-1
ΔP_gF: -0.0028
climatic_resistance: 2.0
stain_resistance: 3.0
acid_resistance: 52.3
alkali_resistance: 1.2
phosphate_resistance: 3.3

Comments

inquiry glass

References

SCHOTT Zemax catalog 2015-07-22

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SCHOTT AG

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.

External links


Glass

External links