RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - Inquiry glasses
N-BAF3

Wavelength: µm
 (0.365 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.34859634λ^2}{λ^2-0.00871492932}+\frac{0.10764424λ^2}{λ^2-0.0478406436}+\frac{1.13207084λ^2}{λ^2-112.936116}$$

Comments

inquiry glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 1.4e-06 1.24e-08 -9.39e-12 5.91e-07 7.44e-10 0.235
n_d: 1.58272
V_d: 46.64
glass_code: 583466.279
glass_status: special
density: 2.792 g/cm3
coefficient_of_thermal_expansion_1: 7.17e-06 K-1
coefficient_of_thermal_expansion_2: 8.24e-06 K-1
ΔP_gF: 0.0015
climatic_resistance: 1.0
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 1.0
phosphate_resistance: 1.0

References

SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.