Optical constants of SCHOTT - Inquiry glasses
K5G20

Wavelength: µm
 (0.37 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.14094396λ^2}{λ^2-0.00694945478}+\frac{0.14500119λ^2}{λ^2-0.0310574444}+\frac{37.4705786λ^2}{λ^2-4536.25624}$$

Comments

inquiry glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -2.22e-06 8.45e-09 -3.31e-11 5.44e-07 4.95e-10 0.214
n_d: 1.52344
V_d: 56.76
glass_code: 523568.259
glass_status: special
density: 2.593 g/cm3
coefficient_of_thermal_expansion_1: 8.99e-06 K-1
coefficient_of_thermal_expansion_2: 1.028e-05 K-1
ΔP_gF: 0.0017
stain_resistance: 0.0
acid_resistance: 1.0
alkali_resistance: 1.0

References

SCHOTT Zemax catalog 2015-07-22