Optical constants of SCHOTT - Inquiry glasses
FK3

Wavelength: µm
 (0.3 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{0.973346627λ^2}{λ^2-0.00640795469}+\frac{0.146642231λ^2}{λ^2-0.020565293}+\frac{0.679304225λ^2}{λ^2-80.4965389}$$

Comments

inquiry glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: -4.9e-06 1.23e-08 -1.19e-10 3.45e-07 7.72e-10 0.18
n_d: 1.4645
V_d: 65.77
glass_code: 464658.227
glass_status: special
density: 2.27 g/cm3
coefficient_of_thermal_expansion_1: 8.2e-06 K-1
coefficient_of_thermal_expansion_2: 9.4e-06 K-1
ΔP_gF: -0.0003
climatic_resistance: 2.0
stain_resistance: 3.0
acid_resistance: 52.4
alkali_resistance: 2.0
phosphate_resistance: 1.0

References

SCHOTT Zemax catalog 2015-07-22