BAFN6

Wavelength: µm
 (0.35 – 2.325)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.36719201λ^2}{λ^2-0.00882820704}+\frac{0.10907994λ^2}{λ^2-0.0438731646}+\frac{1.02108011λ^2}{λ^2-113.58602}$$

Comments

inquiry glass

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 1.34e-06 1.34e-08 -5.5e-11 4.95e-07 3.62e-10 0.265
n_d: 1.589
V_d: 48.45
glass_code: 589485.317
glass_status: special
density: 3.17 g/cm3
coefficient_of_thermal_expansion_1: 7.8e-06 K-1
coefficient_of_thermal_expansion_2: 8.5e-06 K-1
ΔP_gF: 0.0002
climatic_resistance: 2.0
stain_resistance: 0.0
acid_resistance: 2.0
alkali_resistance: 2.0
phosphate_resistance: 1.0