RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SCHOTT - SF (Dense flint)
SF6HT

Wavelength: µm
 (0.365 – 2.5)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.72448482λ^2}{λ^2-0.0134871947}+\frac{0.390104889λ^2}{λ^2-0.0569318095}+\frac{1.04572858λ^2}{λ^2-118.557185}$$

Comments

lead containing glass type

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: false
λ_is_vacuum: false
temperature: 20.0 °C
coefficients_of_thermal_dispersion: 6.69e-06 1.78e-08 -3.36e-11 1.77e-06 1.7e-09 0.269
n_d: 1.80518
V_d: 25.43
glass_code: 805254.518
glass_status: standard
density: 5.18 g/cm3
coefficient_of_thermal_expansion_1: 8.1e-06 K-1
coefficient_of_thermal_expansion_2: 9e-06 K-1
ΔP_gF: 0.0092
climatic_resistance: 2.0
stain_resistance: 3.0
acid_resistance: 51.3
alkali_resistance: 2.3
phosphate_resistance: 3.3

References

1) SCHOTT optical glass data sheets 2015-07-22
2) SCHOTT Zemax catalog 2015-07-22

More info - wiki

SCHOTT AG is a German glass manufacturer. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.