Optical constants of Pilkington-Optiwhite (NSG)
Treharne et al. 2011: n,k 0.3–1.5 µm
Wavelength:
µm
(0.30141754–1.4979382)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Variable-angle ellipsometer was used to take amplitude and phase change measurements. The refractive index and extinction coefficient was extracted for NSG Opti-White (low-Fe) glass from a multi-oscillator model fit to the ellipsometry data, as a function of wavelength, from 300 to 1500 nm
References
R. E. Treharne. RF magnetron sputtering of transparent conducting oxides and CdTe/CdS solar cells. PhD Thesis, University of Durham (2011) (Numerical data kindly provided by Dr. Robert Treharne)