Optical constants of OHARA - i-Line glasses
PBM8Y

Wavelength: µm
 (0.32 – 2.4)  
 

Derived optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.35351322λ^2}{λ^2-0.0105624626}+\frac{0.130212912λ^2}{λ^2-0.0496606652}+\frac{0.158337266λ^2}{λ^2-20.7965806}$$

Conditions & Spec sheet

n_is_absolute: false
λ_is_vacuum: false
temperature: 25.0 °C
coefficients_of_thermal_dispersion: 6.76e-07 1.49e-08 -3.72e-11 9.2e-07 8.07e-10 0.227
n_d: 1.595509
V_d: 39.260208
glass_code: 596393
density: 3.36 g/cm3
coefficient_of_thermal_expansion_1: 8.5e-06 K-1
coefficient_of_thermal_expansion_2: 9.6e-06 K-1
ΔP_gF: -0.0012
climatic_resistance: 1.0
acid_resistance: 1.0
phosphate_resistance: 2.0

Comments

Improved XMT at 365

References

1) OHARA i-line glass data
2) OHARA Zemax catalog 2015-12-01

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Ohara Group

Ohara Group is an international group of companies with headquarters in Japan and subsidiaries in Japan (Ohara, Inc.), United States (Ohara Corporation), and Germany (Ohara, GmbH). Ohara manufactures optical and electronic products and also offers measurement services, in particular measurement of refractive indices of solids and liquids.

External links


Glass

External links