RefractiveIndex.INFO

Refractive index database

Shelf

Book

Page

Optical constants of HOYA - NbFD (Dense niobium flint)
M-NBFD82

Wavelength: µm
 (0.35 – 0.7)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.1880260-1.2178420\text{×}10^{-2}λ^{2}+3.7193080\text{×}10^{-2}λ^{-2}-2.8175310\text{×}10^{-4}λ^{-4}+1.8044800\text{×}10^{-4}λ^{-6}-4.1829090\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

HOYA Optical Glass Master Datasheet

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

HOYA Corporation

Hoya Corporation is a Japanese company manufacturing optical products.

External links


Glass