Optical constants of HOYA - NbF (Niobium flint)
NBF2

Wavelength: µm
 (0.3 – 1.55)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.0170177-1.3625149\text{×}10^{-2}λ^{2}+2.4142489\text{×}10^{-2}λ^{-2}+5.9520693\text{×}10^{-4}λ^{-4}-1.2146589\text{×}10^{-5}λ^{-6}+1.4445534\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

HOYA Optical Glass Master Datasheet

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]