Optical constants of HOYA - FD (Dense flint)
M-FD60

Wavelength: µm
 (0.38 – 1.55)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.1180310-1.4855230\text{×}10^{-2}λ^{2}+4.2180350\text{×}10^{-2}λ^{-2}+2.9145800\text{×}10^{-3}λ^{-4}-1.7197010\text{×}10^{-4}λ^{-6}+3.0449950\text{×}10^{-5}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

HOYA Optical Glass Master Datasheet

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]