Optical constants of HOYA - ADC (Abnormal dispersion crown)
ADC1

Wavelength: µm
 (0.32 – 0.7)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.5823900-7.8947925\text{×}10^{-3}λ^{2}+1.4967726\text{×}10^{-2}λ^{-2}+1.4902926\text{×}10^{-4}λ^{-4}+4.6409361\text{×}10^{-6}λ^{-6}+2.1550228\text{×}10^{-7}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

HOYA Optical Glass Master Datasheet

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]