Optical constants of CDGM - ZLAF (Dense lanthanum flint)
H-ZLAF50B

Wavelength: µm
 (0.365 – 0.7065)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.1767027-1.5350032\text{×}10^{-2}λ^{2}+2.6690666\text{×}10^{-2}λ^{-2}+7.0784089\text{×}10^{-4}λ^{-4}-1.5485093\text{×}10^{-5}λ^{-6}+1.9530666\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers