Optical constants of CDGM - ZBAF (Dense barium flint)
ZBAF1

Wavelength: µm
 (0.365 – 0.7065)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.5835857-8.9093372\text{×}10^{-3}λ^{2}+1.6695868\text{×}10^{-2}λ^{-2}+3.7304559\text{×}10^{-4}λ^{-4}-8.6297573\text{×}10^{-6}λ^{-6}+1.0908659\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

CDGM Optical Glass Products Database

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]