RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of CDGM - LAK (Lanthanum crown)
H-LAK7

Wavelength: µm
 (0.365 – 0.7065)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.8747114-1.2071704\text{×}10^{-2}λ^{2}+2.228392\text{×}10^{-2}λ^{-2}-2.9355832\text{×}10^{-4}λ^{-4}+8.2863813\text{×}10^{-5}λ^{-6}-3.5482876\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CDGM Optical Glass Products Database

More info - wiki

-