Optical constants of CDGM - LAK (Lanthanum crown)
H-LAK50

Wavelength: µm
 (0.365 – 0.7065)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.6876223-1.4375187\text{×}10^{-2}λ^{2}+1.2545954\text{×}10^{-2}λ^{-2}+1.4642295\text{×}10^{-3}λ^{-4}-1.6982461\text{×}10^{-4}λ^{-6}+8.8048639\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CDGM Optical Glass Products Database