Optical constants of CDGM - D- (Low softening glass)
D-LAK70

Wavelength: µm
 (0.365 – 0.7065)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.7351361-1.1822071\text{×}10^{-2}λ^{2}+1.8279111\text{×}10^{-2}λ^{-2}+1.7985842\text{×}10^{-4}λ^{-4}+1.6773012\text{×}10^{-5}λ^{-6}-5.3070611\text{×}10^{-7}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

CDGM Optical Glass Products Database