Optical constants of CDGM - BAF (Barium flint)
BAF6

Wavelength: µm
 (0.365 – 0.7065)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.5302155-7.6369172\text{×}10^{-3}λ^{2}+1.9460977\text{×}10^{-2}λ^{-2}+7.9936292\text{×}10^{-5}λ^{-4}+4.7154385\text{×}10^{-5}λ^{-6}-8.474266\text{×}10^{-7}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CDGM Optical Glass Products Database