Optical constants of CDGM - BAF (Barium flint)
BAF3

Wavelength: µm
 (0.365 – 0.7065)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.4533945-9.2170291\text{×}10^{-3}λ^{2}+1.4211471\text{×}10^{-2}λ^{-2}+5.2262954\text{×}10^{-4}λ^{-4}-3.2362906\text{×}10^{-5}λ^{-6}+2.1397007\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

References

CDGM Optical Glass Products Database