Optical constants of Ag (Silver)
Johnson and Christy 1972: n,k 0.188–1.94 µm

Wavelength: µm
 (0.1879–1.9370)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Room temperature

References

P. B. Johnson and R. W. Christy. Optical constants of the noble metals, Phys. Rev. B 6, 4370-4379 (1972)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]