lambda,n,k 0.200,1.396,1.10E-7 0.225,1.373,4.90E-8 0.250,1.362,3.35E-8 0.275,1.354,2.35E-8 0.300,1.349,1.60E-8 0.325,1.346,1.08E-8 0.350,1.343,6.50E-9 0.375,1.341,3.50E-9 0.400,1.339,1.86E-9 0.425,1.338,1.30E-9 0.450,1.337,1.02E-9 0.475,1.336,9.35E-10 0.500,1.335,1.00E-9 0.525,1.334,1.32E-9 0.550,1.333,1.96E-9 0.575,1.333,3.60E-9 0.600,1.332,1.09E-8 0.625,1.332,1.39E-8 0.650,1.331,1.64E-8 0.675,1.331,2.23E-8 0.700,1.331,3.35E-8 0.725,1.330,9.15E-8 0.750,1.330,1.56E-7 0.775,1.330,1.48E-7 0.800,1.329,1.25E-7 0.825,1.329,1.82E-7 0.850,1.329,2.93E-7 0.875,1.328,3.91E-7 0.900,1.328,4.86E-7 0.925,1.328,1.06E-6 0.950,1.327,2.93E-6 0.975,1.327,3.48E-6 1.0,1.327,2.89E-6 1.2,1.324,9.89E-6 1.4,1.321,1.38E-4 1.6,1.317,8.55E-5 1.8,1.312,1.15E-4 2.0,1.306,1.10E-3 2.2,1.296,2.89E-4 2.4,1.279,9.56E-4 2.6,1.242,3.17E-3 2.65,1.219,6.70E-3 2.70,1.188,0.019 2.75,1.157,0.059 2.80,1.142,0.115 2.85,1.149,0.185 2.90,1.201,0.268 2.95,1.292,0.298 3.00,1.371,0.272 3.05,1.426,0.240 3.10,1.467,0.192 3.15,1.483,0.135 3.20,1.478,0.0924 3.25,1.467,0.0610 3.30,1.450,0.0368 3.35,1.432,0.0261 3.40,1.420,0.0195 3.45,1.410,0.0132 3.50,1.400,0.0094 3.6,1.385,0.00515 3.7,1.374,0.00360 3.8,1.364,0.00340 3.9,1.357,0.00380 4.0,1.351,0.00460 4.1,1.346,0.00562 4.2,1.342,0.00688 4.3,1.338,0.00845 4.4,1.334,0.0103 4.5,1.332,0.0134 4.6,1.330,0.0147 4.7,1.330,0.0157 4.8,1.330,0.0150 4.9,1.328,0.0137 5.0,1.325,0.0124 5.1,1.322,0.0111 5.2,1.317,0.0101 5.3,1.312,0.0098 5.4,1.305,0.0103 5.5,1.298,0.0116 5.6,1.289,0.0142 5.7,1.277,0.0203 5.8,1.262,0.0330 5.9,1.248,0.0622 6.0,1.265,0.107 6.1,1.319,0.131 6.2,1.363,0.0880 6.3,1.357,0.0570 6.4,1.347,0.0449 6.5,1.339,0.0392 6.6,1.334,0.0356 6.7,1.329,0.0337 6.8,1.324,0.0327 6.9,1.321,0.0322 7.0,1.317,0.0320 7.1,1.314,0.0320 7.2,1.312,0.0321 7.3,1.309,0.0322 7.4,1.307,0.0324 7.5,1.304,0.0326 7.6,1.302,0.0328 7.7,1.299,0.0331 7.8,1.297,0.0335 7.9,1.294,0.0339 8.0,1.291,0.0343 8.2,1.286,0.0351 8.4,1.281,0.0361 8.6,1.275,0.0372 8.8,1.269,0.0385 9.0,1.262,0.0399 9.2,1.255,0.0415 9.4,1.247,0.0433 9.6,1.239,0.0454 9.8,1.229,0.0479 10.0,1.218,0.0508 10.5,1.185,0.0662 11.0,1.153,0.0968 11.5,1.126,0.142 12.0,1.111,0.199 12.5,1.123,0.259 13.0,1.146,0.305 13.5,1.177,0.343 14.0,1.210,0.370 14.5,1.241,0.388 15.0,1.270,0.402 15.5,1.297,0.414 16.0,1.325,0.422 16.5,1.351,0.428 17.0,1.376,0.429 17.5,1.401,0.429 18.0,1.423,0.426 18.5,1.443,0.421 19.0,1.461,0.414 19.5,1.476,0.404 20.0,1.480,0.393 21.0,1.487,0.382 22,1.500,0.373 23,1.511,0.367 24,1.521,0.361 25,1.531,0.356 26,1.539,0.350 27,1.545,0.344 28,1.549,0.338 29,1.551,0.333 30,1.551,0.328 32,1.546,0.324 34,1.536,0.329 36,1.527,0.343 38,1.522,0.361 40,1.519,0.385 42,1.522,0.409 44,1.530,0.436 46,1.541,0.462 48,1.555,0.488 50,1.587,0.514 60,1.703,0.587 70,1.821,0.576 80,1.886,0.547 90,1.924,0.536 100,1.957,0.532 110,1.966,0.531 120,2.004,0.526 130,2.036,0.514 140,2.056,0.500 150,2.069,0.495 160,2.081,0.496 170,2.094,0.497 180,2.107,0.499 190,2.119,0.501 200,2.130,0.504