Optical constants of Si₃N₄ (Silicon nitride)

From RefrectiveIndex.INFO - Refractive index database

Optical constants of Si3N4 (Silicon nitride)
Wavelength: µm  (0.207~1.24)
Refractive index

Refractive index - Wikipedia

n = 2.01673

Chromatic dispersion

Dispersion (optics) - Wikipedia

dn/dλ = -0.155 µm-1

Abbe numbers

Abbe number - Wikipedia

Vd = 33.42

Ve = 33.23

Formulae    Abbe diagram

[ Figure: Refractive index of Si3N4 (Silicon nitride) ]
Dispersion formula

Sellmeier equation - Wikipedia

$$ n^2 - 1 = \frac{2.8939 λ^2}{λ^2-139.67\text{×}10^{-3}^2} $$

C

n = sqrt( 1 + 2.8939*pow(x,2)/(pow(x,2)-pow(139.67e-3,2)) )

Fortran

n = SQRT( 1 + 2.8939*x**2/(x**2-139.67e-3**2) )

Visual Basic

n = SQRT( 1 + 2.8939*x**2/(x**2-139.67e-3**2) )

Expressions for n

References

- T. Bååk. Silicon oxynitride; a material for GRIN optics, Appl. Optics 21, 1069-1072 (1982) doi:10.1364/AO.21.001069

Reflection calculator
Angle of incidence (0~90°): 
Direction: in out
Reflectance (at 0.5876 µm)

Fresnel equations - Wikipedia

RS = ... (S-polarized)
RP = ... (P-polarized)
R = ... (non-polarized, (RS+RP)/2 )

Reflection phase

ɸ = ...°
ɸS = ...°
ɸP = ...°

Brewster's angle

Brewster's angle - Wikipedia

θB = ...°

Critical angle

Total internal reflection - Wikipedia

θC = ...°

More info ( wiki )

Silicon nitride, Si3N4

External links

© 2008-2013 Mikhail Polyanskiy   |   Link to or cite RefractiveIndex.INFO   |   NO GUARANTEE OF ACCURACY - Use on your own risk