RefractiveIndex.INFO Refractive index database |
|
Refractive index at 0.5876 µm
n = 1.4914 dn/dλ at 0.5876 µm
dn/dλ = -0.0575 µm-1 Abbe numbers
Vd = 52.60 Ve = 53.85 |
Chromatic dispersion curve
Dispersion (optics) - Wikipedia
|
n2 = C1 + C2λ2 + C3λ-2 + C4λ-4 + C5λ-6 + C6λ-8
C1 = 2.399964; C2 = -8.308636E-2; C3 = -1.919569E-1; C4 = 8.720608E-2; C5 = -1.666411E-2; C6 = 1.169519E-3
Angle of incidence (0~90°):
Direction: in out
20 °C
S. N. Kasarova et al. Analysis of the dispersion of optical plastic materials, Optical Materials 29, 1481-1490 (2007) [doi:10.1016/j.optmat.2006.07.010]
Molecular formula: (C5O2H9)n. Trademarks: Plexiglas, Vitroflex, Limacryl, R-Cast, Per-Clax, Perspex, Plazcryl, Acrylex, Acrylite, Acrylplast, Altuglas, Polycast, Oroglass, Lucite.