Brewster's angle of FUSED SILICA for λ = 0.5876 µm, entering beam:

θB = 55.563°

Reflection coefficients as functions of angle of incidence:

[ Figure: Reflection coefficient of FUSED SILICA ]

Calculated using refractive index data from Refractive index database