Micro resist EpoCore

Wavelength: µm
 (0.45 – 1.55)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.572+0.0076λ^{-2}+0.00046λ^{-4}$$

Comments

Micro resist EpoCore negative photoresist for waveguide manufacturing

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Micro resist EpoCore and EpoClad datasheet, 2015

More info - wiki