Optical constants of Fused silica matching liquid
Cargille-50350

Wavelength: µm
 (0.225 – 1.55)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.446902+398962.9\text{×}10^{-8}λ^{-2}+3.757747\text{×}10^{-5}λ^{-4}$$

Comments

Code 50350 (viscosity 19 cSt). 25 °C.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CARGILLE Fused Silica matching liquid (code 50350) characteristics. Jan. 15, 2002

More info - wiki

An index-matching material is usually used to create an optical contact with minimum reflection between optical components.