RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Acrylic matching liquid
Cargille

Wavelength: µm
 (0.31 – 1.55)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.478419+463182.1\text{×}10^{-8}λ^{-2}-8.637338\text{×}10^{-6}λ^{-4}$$

Comments

25 °C

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CARGILLE Acrylic matching liquid characteristics. August 10, 2004

More info - wiki

An index-matching material is usually used to create an optical contact with minimum reflection between optical components.

External links