Optical constants of Acetylene soot
Dalzell and Sarofim 1969: n,k 0.4358-10 µm

Wavelength: µm
 (0.4358 – 10.0)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Room temperature

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

W. H. Dalzell and A. F. Sarofim. Optical constants of soot and their application to heat-flux calculations, J. Heat Transfer 91, 100-104 (1969)