Optical constants of ZrO2-Y2O3 (Yttria-stabilized zirconia, YSZ)
Wood and Nassau 1982: 12 mol % Y2O3; n 0.361-5.135 µm

Wavelength: µm
 (0.361 – 5.135)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.347091λ^2}{λ^2-0.062543^2}+\frac{2.117788λ^2}{λ^2-0.166739^2}+\frac{9.452943λ^2}{λ^2-24.320570^2}$$

Comments

Cubic zirconiza; 25 °C; Y2O3 content: 12.0 mol %

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. L Wood and K. Nassau. Refractive index of cubic zirconia stabilized with yttria, Appl. Opt. 21, 2978-2981 (1982)