Optical constants of Optical adhesives
Norland NOA 61

Wavelength: µm
 (0.45 – 1.55)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.5375+0.00829045λ^{-2}-0.000211046λ^{-4}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Norland Optical Adhesive 61 Data 1, Data 2 (accessed 2016-04-20)

More info - wiki

Optical Adhesives are used to bond or cement optical components together (from Edmund Optics)