Optical constants of Nb-Sn (Niobium-tin alloy)
Golovashkin et al. 1971: n,k 1-10 µm; 28 wt% Sn

Wavelength: µm
 (1.0 – 10.0)  
 

Other optical constants

n   k   logX   logY   eV

Comments

28 wt% Sn; room temperature.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. I. Golovashkin, E. D. Donner, I. S. Levchenko, G. P. Motulevich. Optical properties and electronic characteristics of alloys of niobium with tin, Sov. Phys. JETP 32, 1064-1067 (1971)